Basic Performance Comparison | ||
Testing items | SF300 | SF180MR |
The lowest curing temperature℃ (after 4 seconds) |
170℃ | 160℃ |
Subsequent Adhesion % | 92.5 | 93.8 |
RF-RT(g/in) | 7.2 | 9.0 |
RF-70(g/in) | 17.1 | 19.7 |
Note: RF=release force; RF—RT= Release force @ room temperature; RF—70=Stable release force; Testing speed (lower) 0.3m/min;Testing tape: tesa7475; Coating paper: Glassine |
Actual anti-misting data under machine Speed 500m/min | |||
Products | Working side(mg/m3 ) | Middle(mg/m3 ) | Driving side(mg/m3 ) |
SF300 | 1.32 | 1.1 | 1.25 |
SF180MR | 0.325 | 0.217 | 0.255 |
Competitor | 0.657 | 0.431 | 0.512 |
SF180MR shows more advantages in high-speed coating, significantly improves the coating environment, and greatly improves the health and environmental protection of personnel. In addition, the release paper and self-adhesive products produced by SF180MR have stable peeling performance, high speed and low peeling effect, which can meet the high-speed labeling requirements of downstream customers.
High speed peeling comparison | |||||
Release force(g/in)- room temperature | 0.3m/min | 30m/min | 100m/min | 150m/min | 300m/min |
SF300 | 7.2 | 88.5 | 138.1 | 148.5 | 152.3 |
SF180MR | 9 | 76.68 | 117.1 | 123.9 | 118.7 |
Competitor | 9.5 | 82.2 | 112.5 | 132.4 | 121.3 |